  • Maintain sharp tools to minimize heat buildup and galling.
  • Good tool life and successful machining of titanium alloys can be assured if the following guidelines are observed: Like stainless steel, the low thermal conductivity of titanium inhibits dissipation of heat within the workpiece itself, thus requiring proper application of coolants. The factors which must be given consideration are not complex, but they are vital to successfully machining titanium.The different grades of titanium, i.e., commercially pure and various alloys, do not have identical machining characteristics, any more than all steels, or all aluminum grades have identical characteristics. Titanium can be economically machined on a routine production basis if shop procedures are set up to allow for the physical characteristics common to the metal. Chemical Analysis of Titanium Grade 17 (weight %) Grade 17 has optimum ductility and cold formability with useful strength, high-impact toughness, and excellent weldability.

    titanum grade for flexture use

    Titanium Grade 17Ti Grade 17, is the same as Grade 1, but with Pd for better corrosion resistance. Has a good balance of moderate strength, reasonable ductility and excellent weldabilityĬhemical Analysis of Titanium Grade 16 (weight %) Titanium Grade 16Ti Grade 16 is corrosion-resistant material offering outstanding resistance to general and localized crevice corrosion in a wide range of oxidizing and reducing acid environments including chlorides. Titanium Grade 12Ti Grade 12 is highly weldable, exhibiting improved strength allowable at increased temperatures, combined with superior crevice corrosion resistance, and excellent resistance under oxidizing to mildly reducing conditions, especially chlorides.Ĭhemical Analysis of Titanium Grade 12 (weight %) It has also useful strength, high-impact toughness and excellent weldability.Ĭhemical Analysis of Titanium Grade 11 (weight %) Grade 11 has optimum ductility and cold formability. Titanium Grade 11Ti Grade 11, is the same as Grade 1, but with Pd for better corrosion resistance.

    #TITANUM GRADE FOR FLEXTURE USE PLUS#

    The alloy has excellent formability plus higher tensile strength than the strongest unalloyed grade.Ĭhemical Analysis of Titanium Alloy Grade 9 (weight %)

    titanum grade for flexture use

    Grade 9 combines strength, weldability and formability. grades, but is more formable and weldable than Ti-6AI-4V. It offers 20-50% higher strength than C.P.

    titanum grade for flexture use

    Titanium Alloy Grade 9Ti Grade 9, is sometimes referred to as “half 6-4″. Physical and mechanical properties equivalent to Grade 2.Ĭhemical Analysis of Titanium Grade 7 (weight %) Titanium Grade 7Ti Grade 7,Most corrosion-resistant titanium alloy offering outstanding resistance to general and localized crevice corrosion in a wide range of oxidizing and reducing acid environments including chlorides, with a good balance of moderate strength, reasonable ductility and excellent weldability. The alloy is weldable and can be precipitation hardened.Ĭhemical Analysis of Titanium Alloy Grade 5 (weight %) The main application of this alloy is in aircraft and spacecraft. Titanium Alloy Grade 5Ti Grade 5 has very high strength but relatively low ductility. Chemical Analysis of CP Titanium Grade 2 (weight %) This titanium also has excellent resistance to high oxidization. CP Titanium Grade 1Ti Grade 1 is the softest titanium with the highest ductility, good cold formability which gives Ti Grade 1 an excellent resistance from mild to high oxidization.Ĭhemical Analysis of CP Titanium Grade 1 (weight %)ĬP Titanium Grade 2Ti Grade 2 has moderate strength with excellent cold formability, weldability.